Journal of the Korean Ceramic Society 1998;35(1): 48.
질화규소 이층 층상재료에서 코팅층의 파괴에 관한 연구 : II Coating Thickness의 영향
이기성, 이승건1, 김도경
한국과학기술원 재료공학과
1미국표준과학연구소
A Study on the Coating Fracture in Silicon Nitride Bilayer : II. Effect of Coating Thickness
ABSTRACT
The effect of coating thickness on the contact fracture was studied, in Si3N4 coated Si3N4-BN system When the elastic/plastic mismatch is relatively large betwen two layers in bilayer certain critical coating thickness was required to prevent cone crack initiation and this critical thickness was decreased by de-creasing the elastic/plastic mismatch,. In addition the required critical thickness should be increased when higher loads apply. In conclusion an appropriate coating thickness should be designed by elastic/plastic mismatch between two layers and environment (applied load) to prevent the coating fracture,
Key words: Coating fracture, Coating thickness, Elastic/Plastic Mismatch, Hertzian indentation
Editorial Office
Meorijae Bldg., Suite # 403, 76, Bangbae-ro, Seocho-gu, Seoul 06704, Korea
TEL: +82-2-584-0185   FAX: +82-2-586-4582   E-mail: ceramic@kcers.or.kr
About |  Browse Articles |  Current Issue |  For Authors and Reviewers
Copyright © The Korean Ceramic Society.                      Developed in M2PI