자체반응열 고온합성법에 의한 $Ti_3AI$ 생상반응의 동력학적 연구
전광식
재능대학 공업화학과
Studies on the Kinetics for the Formation Reaction $Ti_3AI$ by SHS (Self-propagating High-temperatuer Synthesis) Method
ABSTRACT
The thickness of flame zone reaction rate and apparent activation energy in the formation reaction of $Ti_3AI$ intermetallic compound were investigated using SHS method which sustains the reaction spontaneously and utilizes the heat generated by thye exothermic reaction itself. In this reaction the thickness of flame zone was 1.4 mm and the reaction rate was $0.4g/textrm{cm}^2{cdot}sec$. Also the apparent activation energy calculated using from the experimental data obtained by controlling the realtive green density was 40kJ/mol.
Key words: Thickness, Spontaneously, Activation, Density, $Ti_3AI$ intermetallic
Editorial Office
Meorijae Bldg., Suite # 403, 76, Bangbae-ro, Seocho-gu, Seoul 06704, Korea
TEL: +82-2-584-0185   FAX: +82-2-586-4582   E-mail: ceramic@kcers.or.kr
About |  Browse Articles |  Current Issue |  For Authors and Reviewers
Copyright © The Korean Ceramic Society.                      Developed in M2PI