ABSTRACT
Quick hardened property and compressive strength experimented to the C4A3 quantities. Workability experimented to the hydration behavior as retarder added to the C4A3. Compressive strength reached {{{{ delta }}3h=300~350 kgf/$textrm{cm}^2$, {{{{ delta }}6h=400~450 kgf/$textrm{cm}^2$, {{{{ delta }}24h=500~550 kgf/$textrm{cm}^2$. Flow loss rate reached 70.1% to retarder addition 0.12% after 15 min. Test items were SEM, XRD, TG-DTA, MCC, porosity and zeta potential.
Key words: Quick hardened cement mortar grouts, Retarder, Anhydrite
Editorial Office
Meorijae Bldg., Suite # 403, 76, Bangbae-ro, Seocho-gu, Seoul 06704, Korea
TEL: +82-2-584-0185   FAX: +82-2-586-4582   E-mail: ceramic@kcers.or.kr
About |  Browse Articles |  Current Issue |  For Authors and Reviewers
Copyright © The Korean Ceramic Society.                      Developed in M2PI