SiC/$SiO_2$ 계면의 고온 기공발생에 관한 열역학적 계산
이문희, 박종욱1
수원대학교 전자재료과
1한국과학기술원 과학기술대학 전자재료과
Thermodynamic Calculations of High Temperature Bubble Formation at SiC/$SiO_2$ Interface
ABSTRACT
Numerous researchers have observed the bubble fromation at SiC/SiO2 interface from 130$0^{circ}C$ to 1$700^{circ}C$. According to thermodynamic calculation, the bubble could be formed from the microscopic impurities which result from the chemical vapor deposition of SiC. When C-impurity is present at the interface, it is calculated that the bubble is formed at 1511$^{circ}C$ and when Si is present, the bubble is formed at 177$0^{circ}C$. These results are very close to the prior observations, but the calculation can not explain the observation of bubble below 150$0^{circ}C$.
Editorial Office
Meorijae Bldg., Suite # 403, 76, Bangbae-ro, Seocho-gu, Seoul 06704, Korea
TEL: +82-2-584-0185   FAX: +82-2-586-4582   E-mail: ceramic@kcers.or.kr
About |  Browse Articles |  Current Issue |  For Authors and Reviewers
Copyright © The Korean Ceramic Society.                      Developed in M2PI