파인 물라이트 소결체에 대한 연구(II)
김경용, 김윤호, 강선모, 김병호1, 김석수1
한국과학기술연구원 정밀요업실
1고려대학교 재료공학과
Studies on the Fine Sintered Mullite(II)
ABSTRACT
Submicron high-purity mullite powder was prepared by a colloidal sol-gel route. Boehmite and silica were the starting materials. 2wt% $alpha$-Al2O3 or ZrO2 was used as a seeding material. The gelled powder was calcined at 130$0^{circ}C$ for 100min and attrition milled for 3hrs. The mullite powder obtained was composed of submicrometer and uniform particles with a narrow size distribution. It was hot-pressed at 1$600^{circ}C$ for 1hr under 10MPa or was sintered at 1$650^{circ}C$ for 4hrs. The bulk densities of the products made by both processes were 3.14 and 3.12g/㎤. the mechanical, thermal and electrical properties of the sintered mullite were characterized by bending strength, thermal expansion coefficient, thermal conductivity, dielectric constant and dielectric loss, etc.
Editorial Office
Meorijae Bldg., Suite # 403, 76, Bangbae-ro, Seocho-gu, Seoul 06704, Korea
TEL: +82-2-584-0185   FAX: +82-2-586-4582   E-mail: ceramic@kcers.or.kr
About |  Browse Articles |  Current Issue |  For Authors and Reviewers
Copyright © The Korean Ceramic Society.                      Developed in M2PI