High-temperature Oxidation Kinetics and Scales Formed on Fe-2.3%Cr-1.6%W Alloy
Sang-Hwan Bak, Min-Jung Kim, Jae-Ho Lee, Sung-June Bong, Seul-Ki Kim, Dong-Bok Lee
J. Korean Ceram. Soc. 2011;48(1):57     DOI: https://doi.org/10.4191/kcers.2011.48.1.057
Citations to this article as recorded by Crossref logo
Simultaneous thermal analysis of the high-temperature oxidation behaviour of three hot-work tool steels
Tilen Balaško, Maja Vončina, Jožef Medved
Journal of Thermal Analysis and Calorimetry.2023; 148(4): 1251.     CrossRef
High-Temperature Oxidation Behavior of Tool Steel with Increased Thermal Conductivity
Tilen Balaško, Maja Vončina, Jaka Burja, Barbara Šetina Batič, Jožef Medved
Oxidation of Metals.2022; 98(1-2): 135.     CrossRef
High-Temperature Oxidation Behaviour of AISI H11 Tool Steel
Tilen Balaško, Maja Vončina, Jaka Burja, Barbara Šetina Batič, Jožef Medved
Metals.2021; 11(5): 758.     CrossRef
Pseudo-icosahedral Cr55Al232−δ as a high-temperature protective material
R. Rosa, S. Bhattacharya, J. Pabla, H. He, J. Misuraca, Y. Nakajima, A. D. Bender, A. K. Antonacci, W. Adrip, D. E. McNally, A. Zebro, P. Kamenov, G. Geschwind, S. Ghose, E. Dooryhee, A. Ibrahim, T. M. Tritt, M. C. Aronson, J. W. Simonson
Physical Review Materials.2018;[Epub]     CrossRef
Corrosion of Fe-2.25%Cr-1.6%W Steel at 600 and 700℃ in N2/(0.5, 2.5)%H2S-mixed Gas
Dong Bok Lee, Sang Hwan Bak
Journal of the Korean institute of surface engineering.2016; 49(4): 339.     CrossRef