고분자 열분해 방법으로 제조된 TiN-Ti5Si3 세라믹 복합체의 고온 산화 거동
김범섭, 김득중, 이동복
성균관대학교 신소재공학부
High-Temperature Oxidation Behavior of TiN-Ti5Si3 Ceramic Composites Manufactured by Polymer Pyrolysis
Beom-Seob Kim, Deug-Joong Kim, Dong-Bok Lee
School of Materials Science and Engineering, Sungkyunkwan University
ABSTRACT
A new $TiN-Ti_5Si_3$ bulk composite was synthesized from preceramic, inorganic polymer (methylpolysilsesquioxane) and $TiH_2$ filler powders via polymer pyrolysis. Using this process, ceramics with high melting points can be produced relatively easily to a near net shape. The $TiN-Ti_5Si_3$ composite oxidized slowly during heating to $1000^{circ}C$. During heating at the temperatures of at 700 and $800^{circ}C$, TiN oxidized to Rutile-$TiO_2$ whereas $Ti_5Si_3$ resisted to oxidation. The oxide scale formed consisted primarily of $TiO_2$ containing $Ti_5Si_3$.
Key words: TiN, $Ti_5Si_3$, Polymer pyrolysis, $TiO_2$
Editorial Office
Meorijae Bldg., Suite # 403, 76, Bangbae-ro, Seocho-gu, Seoul 06704, Korea
TEL: +82-2-584-0185   FAX: +82-2-586-4582   E-mail: ceramic@kcers.or.kr
About |  Browse Articles |  Current Issue |  For Authors and Reviewers
Copyright © The Korean Ceramic Society.                      Developed in M2PI