Journal of the Korean Ceramic Society 1996;33(2): 192.
타이타니아 단섬유상의 석출이 결정화유리의 마모특성에 미치는 영향
이경호
순천향대학교 재료공학과
Effects of Titania Whisker Precipitation on Wear Property of the Glass-Ceramic
ABSTRACT
In Li0.4Ca0.05AlP0.5Si0.75O4.5 composition glass, glass-ceramic having a near 100% crystallinity after nucleation heat treatment of 74$0^{circ}C$/2 h and crystallization heat treatment of 90$0^{circ}C$/2 h and in-situ TiO2 whisker reinforced glass-ceramic after heat treatment of 105$0^{circ}C$ for 20 h were fabricated with the addition of 4% TiO2 as a nucleating agent. With these materials a ball-on-disc type wear test was conducted in order to examine the effect of TiO2 whisker prepcipitation on ambient and high temperature wear properties of the glass-ceramic. Wear test results indicated that all specimens exhibited micro-fracture wear mechanism in ambient temperature. As temperature increased the wear rates of the materials were increased. However the in-situ TiO2 whisker reinforced glass-ceramic exhibited the lowest wear rate over the test temperature range. This resulted from the improvement of harness and fracture toughness of the material as the glass converted into the glass-ceramic followed by precipitation of TiO2 whiskers throughout the glass-ceramic matrix.
Key words: In-situ glass-ceramic composite, $TiO_2$ whisker precipitation, Wear properties
Editorial Office
Meorijae Bldg., Suite # 403, 76, Bangbae-ro, Seocho-gu, Seoul 06704, Korea
TEL: +82-2-584-0185   FAX: +82-2-586-4582   E-mail: ceramic@kcers.or.kr
About |  Browse Articles |  Current Issue |  For Authors and Reviewers
Copyright © The Korean Ceramic Society.                      Developed in M2PI