ABSTRACT
Textured $Bi_{0.5}(Na,K)_{0.5}TiO_3-BiFeO_3$ ceramics were prepared by the reactive-templated grain growth process, using platelike $Bi_4Ti_3O_{12}$ particles. The effects of chemical composition in $Bi_{0.5}(Na,K)_{0.5}TiO_3$ on texture development and densification were examined. Textured ceramics were obtained by using $Bi_{0.5}K_{0.5}TiO_3$ as an end member of the solid solution but densification was limited. Dense ceramics were obtained by using $Bi_{0.5}Na_{0.5}TiO_3$ but texture did not develop. Dense, textured ceramics were obtained by using $Bi_{0.5}(Na_{0.5}K_{0.5})_{0.5}TiO_3$.
Key words: Texture, Reactive-templated grain growth, Solid solutions, $Bi_{0.5}Na_{0.5}TiO_3$, $Bi_{0.5}K_{0.5}TiO_3$
Editorial Office
Meorijae Bldg., Suite # 403, 76, Bangbae-ro, Seocho-gu, Seoul 06704, Korea
TEL: +82-2-584-0185   FAX: +82-2-586-4582   E-mail: ceramic@kcers.or.kr
About |  Browse Articles |  Current Issue |  For Authors and Reviewers
Copyright © The Korean Ceramic Society.                      Developed in M2PI