Thermodynamic and phase analysis of SiC-nano/microB4C-C composites produced by pressureless sintering method
Behnam Salmany Kozekanan1, Alireza Moradkhani2, Hamidreza Baharvandi1, Naser Ehsani1
1Faculty of Materials and Manufacturing Processes, MalekAshtar University of Technology, Tehran, Iran
2Art and Architecture Faculty, Yadegar-E Imam Khomeini (RAH) Shahre-Rey Branch , Islamic Azad University , Tehran , Iran
Correspondence  Alireza Moradkhani ,Email: moradkhani.a@srbiau.ac.ir
Received: July 3, 2021; Revised: October 27, 2021   Accepted: December 6, 2021.  Published online: March 31, 2022.
ABSTRACT
In this research, thermodynamic and phase analysis of SiC-Nano/microB4C composites with different weight percentages of secondary phase including 0, 0.5, 1, and 2 wt% -nano /microB4C made by pressureless sintering method have been investigated. To this end, 0 and 1 wt% phenolic resin were added to the samples separately as a carbon source (both as a binder and as a carbon additive), respectively. The resulting compounds were milled by a planetary ball mill for 3 h at a speed of 200 rpm. The initial pressing of the samples was performed at 50 MPa and the samples were subjected to pyrolysis at 600 °C. They were then sintered at 2150 °C for 2 h under an argon atmosphere. The results showed that the composite contained SiC-0.5 wt% -nanoB 4 C with the main peak intensity (2θ = 35.58) in phasic analysis using XRD pattern of more than 15,000 units and FWHM equal to 0.0036 which shows that the structure is smaller than the additive mode (FWHM = 0.2210) SiC-0.5 wt% -microB4C. Also, the results of phase analysis using the XRD model show that the use of NanoB4C increases the peak intensity in the phase analysis graph compared to the MicroB4C additive mode. In addition, increasing the wt% -nanoB4C increases the amount of graphitization.
Key words: Phase analysis  · Thermal analysis  · Silicon carbide  · Nanocomposite  · Pressureless sintering
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
Share:      
METRICS
4
Crossref
6
Scopus
911
View
26
Download
Related article
Thermal Shock and Hot Corrosion Resistance of Si3N4 Fabricated by Nitrided Pressureless Sintering  2009 ;46(5)
Editorial Office
Meorijae Bldg., Suite # 403, 76, Bangbae-ro, Seocho-gu, Seoul 06704, Korea
TEL: +82-2-584-0185   FAX: +82-2-586-4582   E-mail: ceramic@kcers.or.kr
About |  Browse Articles |  Current Issue |  For Authors and Reviewers
Copyright © The Korean Ceramic Society.                      Developed in M2PI